Interface strength in glass fibre-polypropylene measured using the fibre pull-out and microdebond methods
Tools
Yang, L. and Thomason, J.L. (2009) Interface strength in glass fibre-polypropylene measured using the fibre pull-out and microdebond methods. In: 17th International Conference on Composite Materials, ICCM17, 2009-07-27 - 2009-07-31.
Preview |
Text.
Filename: strathprints008096.pdf
Accepted Author Manuscript Download (784kB)| Preview |
Abstract
Interface strength in glass fibre-polypropylene was measured using both fibre pull-out and microdebond methods. Excellent compatibility between two methods was obtained. The data from microdebond test could be divided into two groups according to whether or not there was constant interfacial friction after debonding.
ORCID iDs
Yang, L. ORCID: https://orcid.org/0000-0001-8475-1757 and Thomason, J.L. ORCID: https://orcid.org/0000-0003-0868-3793;-
-
Item type: Conference or Workshop Item(Paper) ID code: 8096 Dates: DateEvent28 July 2009PublishedSubjects: Technology > Mechanical engineering and machinery Department: Faculty of Engineering > Mechanical and Aerospace Engineering Depositing user: Ms Katrina May Date deposited: 05 Jun 2009 12:30 Last modified: 11 Nov 2024 16:20 URI: https://strathprints.strath.ac.uk/id/eprint/8096